- Micrograph no
- 137
- Brief description
- Al-Mg-Si, failed through microvoid coalescence.
- Keywords
- alloy
, aluminium
, ductile
, fracture
, metal, microvoid coalescence 
- Categories
- Fracture, Metal or alloy
- System
- Al-Mg-Si
- Composition
- Al, Si 1.2, Mg 0.4 (wt%) (AA6016)
- Standard codes
- Reaction
- Processing
- Heat treated at 180 °C for 10 minutes.
- Applications
- Automotive body sheet.
- Sample preparation
- Technique
- Scanning electron microscopy (SEM)
- Length bar
- 40 μm
- Further information
- The rough fracture surface indicates that ductile failure has occurred by microvoid coalescence.
- Contributor
- K Clark
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 24/01/02