137
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
138
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
139
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
140
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
141
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
142
:
Tough pitch copper, failed by fibrous ductile fracture. System: Cu, Composition: Tough pitch copper Scanning electron microscopy (SEM) 20 μm |
![]() |
Micrograph
593
:
Ductile tearing near a fracture surface in polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 100 μm |
![]() |
Micrograph
780
:
Heat treated spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
781
:
Heat treated spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
782
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |