5 micrographs for composition Al, Si 1.2, Mg 0.4 (wt%) (AA6016), ordered by micrograph number.
![]() |
Micrograph
137
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
138
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
139
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
140
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
141
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |