Micrograph
156
:
Roll-bonded aluminium alloy diffusion couple annealed for 30 minutes at 600ºC. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 400 μm |
![]() |
Micrograph
157
:
Roll-bonded aluminium alloy diffusion couple annealed for 60 minutes at 600ºC. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 750 μm |
![]() |
Micrograph
158
:
Roll-bonded aluminium alloy diffusion couple in the as-rolled condition. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 400 μm |
![]() |
Micrograph
159
:
Roll-bonded aluminium alloy diffusion couple in the as-rolled condition. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 2 mm |
![]() |
Micrograph
710
:
Wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute); refined with TiB2 particles. Deformation of grain structure is due to cutting of sample with scissors. System: Al-Mg-Fe-Si, Composition: Not specified Cross-polarised light microscopy 400 μm |
![]() |
Micrograph
711
:
As-cast wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute). No addition of grain refinement particles (e.g. TiB2). System: Al-Mg-Fe-Si, Composition: Not specified Cross-polarised light microscopy 1 mm |
![]() |
Micrograph
712
:
As-cast wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute). Addition of TiB2 particles facilitates the formation of a fine, equiaxed grain structure (grain refinement). System: Al-Mg-Fe-Si, Composition: Not specified Cross-polarised light microscopy 400 μm |