Link to full record for micrograph 818 Micrograph 818 : Austenitic stainless steel tempered
System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Nb 2.5, C 0.1 (wt%)
Scanning electron microscopy (SEM)
4 μm
Link to full record for micrograph 819 Micrograph 819 : Austenitic stainless steel water quenched then deformed in impact
System: Fe-C-X, Composition: Stainless steel with Cr 13.7, Mn 14.2, C 0.12 (wt%)
Reflected light microscopy
50 μm
Link to full record for micrograph 820 Micrograph 820 : Austenitic stainless steel tempered
System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Nb 5, C O.1 (wt%)
Scanning electron microscopy (SEM)
4 μm
Link to full record for micrograph 821 Micrograph 821 : Austenitic stainless steel impact deformed at room temperature
System: Fe-C-X, Composition: Fe, C 1.15, Mn 13 (wt%)
Scanning electron microscopy (SEM)
2.5 μm
Link to full record for micrograph 822 Micrograph 822 : Austenitic stainless steel tempered
System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%)
Transmission electron microscopy (TEM)
400 nm
Link to full record for micrograph 823 Micrograph 823 : Martensitic steel tempered, with dislocation helices in ferrite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 824 Micrograph 824 : Martensitic steel tempered, with precipitation of Mo2C in ferrite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 826 Micrograph 826 : Austenitic stainless steel tempered, with Mo2 and M6C precipitates
System: Fe-C-X, Composition: Fe, C 0.20, Mo 3.8, Ta 0.22 (wt%)
Scanning electron microscopy (SEM)
2.5 μm
Link to full record for micrograph 827 Micrograph 827 : Martensitic steel quenched then tempered
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 828 Micrograph 828 : Martensitic steel tempered, with precipitation of Mo2C on dislocations in ferrite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
500 nm

Showing 301 - 310 of 330 micrographs Page 1 .. 27 28 29 30 31 32 33 | Previous | Next

Help is available on browsing.

Alternatively, search the Library (from top right on any page), or use advanced search.