Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Full Record for Micrograph 827
- Micrograph no
- 827
- Brief description
- Martensitic steel quenched then tempered
- Keywords
- martensite

- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Fe, C 0.2, Mo 4 (wt%)
- Standard codes
- Reaction
- Processing
- Alloy quenched then tempered 90 hours at 550ºC
- Applications
- Sample preparation
- Thin film
- Technique
- Transmission electron microscopy (TEM)
- Length bar
- 1 μm
- Further information
- Contributor
- Professor Sir R W K Honeycombe
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 07/01/04
- Licence for re-use
DoITPoMS standard terms of use