Link to full record for micrograph 27 Micrograph 27 : Fe, C 0.9 (wt%), martensite
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 28 Micrograph 28 : Fe, C 0.9 (wt%), martensite
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Scanning electron microscopy (SEM)
10 μm
Link to full record for micrograph 45 Micrograph 45 : Fe, Ni 30, C 0.3 (wt%), quenched - martensite plates
System: Fe-C-X, Composition: Fe, C 0.3, Ni 30 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 46 Micrograph 46 : Fe, Ni 30, C 0.3 (wt%), quenched - martensite plates
System: Fe-C-X, Composition: Fe, C 0.3, Ni 30 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 278 Micrograph 278 : Fe, C 2, Mn 0.7 (wt%) steel, quenched, producing martensite
System: Fe-C-X, Composition: Fe, C 0.55, Mn 0.65 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 279 Micrograph 279 : Fe, C 2, Mn 0.7 (wt%) steel, quenched, producing martensite and cracking
System: Fe-C-X, Composition: Fe, C 0.55, Mn 0.65 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 280 Micrograph 280 : Fe, C 2, Mn 0.7 (wt%) steel, quenched, producing martensite and cracking
System: Fe-C-X, Composition: Fe, C 0.55, Mn 0.65 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 290 Micrograph 290 : Fe, C 0.4 (wt%) steel, quenched, martensitic and quench cracks
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 291 Micrograph 291 : Fe, C 0.4 (wt%) steel, quenched, martensitic and quench cracks
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 292 Micrograph 292 : Fe, C 0.4 (wt%) steel, quenched, martensitic and quench cracks
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
200 μm