- Micrograph no
- 28
- Brief description
- Fe, C 0.9 (wt%), martensite
- Keywords
- alloy
, carbon, iron, martensite
, metal, steel 
- Categories
- Metal or alloy
- System
- Fe-C-X
- Composition
- Fe, C 0.9 (wt%)
- Standard codes
- Reaction
- Processing
- Water quenched from 800 °C
- Applications
- Sample preparation
- Etched in 3% nital
- Technique
- Scanning electron microscopy (SEM)
- Length bar
- 10 μm
- Further information
- This SEM image of the martensite microstructure clearly shows the intermingled laths.
- Contributor
- Prof T W Clyne
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 25/10/01
- Licence for re-use