Browse the Library
Categories > Metal or alloy > Fe-C-X > Scanning electron microscopy (SEM) > Keyword: stainless steel
12 micrographs available, ordered by micrograph number.
Showing 1 - 10 of 12 micrographs | Page 1 2 | Previous | Next |
Micrograph
799
:
Austenitic stainless steel solution treated, water quenched and tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Scanning electron microscopy (SEM) 2 μm |
|
Micrograph
800
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Nb 1 (wt%) Scanning electron microscopy (SEM) 1 μm |
|
Micrograph
804
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Mo 2.5, C 0.25 (wt%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
805
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, V 5, C 0.1 (wt%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
811
:
Austenitic stainless steel rapidly cooled, fracture surface of laboratory ingot System: Fe-C-X, Composition: Fe, C 0.13, Ni 4, Cr 2, Mn 0.49, S 0.015 (wt%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
812
:
Austenitic stainless steel rapidly cooled, fracture surface of laboratory ingot System: Fe-C-X, Composition: Fe, C 0.13, Ni 4, Cr 2, Mn 0.49, S 0.015 (wt%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
817
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Ti 5, C 0.1 Scanning electron microscopy (SEM) 2 μm |
|
Micrograph
818
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Nb 2.5, C 0.1 (wt%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
820
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Nb 5, C O.1 (wt%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
821
:
Austenitic stainless steel impact deformed at room temperature System: Fe-C-X, Composition: Fe, C 1.15, Mn 13 (wt%) Scanning electron microscopy (SEM) 2.5 μm |