Categories > Metal or alloy > Cu-Sn > Not specified > Keyword: metal

4 micrographs available, ordered by micrograph number.


Link to full record for micrograph 534 Micrograph 534 : Cu - Sn, cast annealed
System: Cu-Sn, Composition: Not specified
Reflected light microscopy
800 μm
Link to full record for micrograph 535 Micrograph 535 : Cu - Sn, cast annealed
System: Cu-Sn, Composition: Not specified
Reflected light microscopy
400 μm
Link to full record for micrograph 536 Micrograph 536 : Cu - Sn, cast annealed
System: Cu-Sn, Composition: Not specified
Reflected light microscopy
200 μm
Link to full record for micrograph 537 Micrograph 537 : Cu - Sn, cast annealed
System: Cu-Sn, Composition: Not specified
Reflected light microscopy
100 μm