Full Record for Micrograph 536
[189 KB]
View micrograph
.. in new window
View micrograph and record
.. in new window
You can also view and download the micrographs on Flickr
- Micrograph no
- 536
- Brief description
- Cu - Sn, cast annealed
- Keywords
- alloy
, bronze
, copper, metal, tin - Categories
- Metal or alloy
- System
- Cu-Sn
- Composition
- Not specified
- Standard codes
- Reaction
- Processing
- Cast annealed
- Applications
- Sample preparation
- Ferric chloride
- Technique
- Reflected light microscopy
- Length bar
- 200 μm
- Further information
- Bronze that has been cast and annealed to give a microstructure with an a matrix surrounded by a mixture of a and b phases
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds
- Date
- 04/09/02