Categories > Metal or alloy > Al-Cu > Reflected light microscopy

18 micrographs available, ordered by micrograph number.


Showing 1 - 10 of 18 micrographs Page 1 2 | Previous | Next

Link to full record for micrograph 1 Micrograph 1 : Al 75, Cu 25 (wt%), hypoeutectic alloy
System: Al-Cu, Composition: Al 75, Cu 25 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 3 Micrograph 3 : Al 67, Cu 33 (wt%), eutectic alloy
System: Al-Cu, Composition: Al 67, Cu 33 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 5 Micrograph 5 : Al 64, Cu 36 (wt%), hypereutectic alloy
System: Al-Cu, Composition: Al 64, Cu 36 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 47 Micrograph 47 : Al 95, Cu 5 (wt%), microsegregation - cored dendrites
System: Al-Cu, Composition: Al 95, Cu 5 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 48 Micrograph 48 : Al 95, Cu 5 (wt%), microsegregation - cored dendrites
System: Al-Cu, Composition: Al 95, Cu 5 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 56 Micrograph 56 : Al 96, Cu 4 (wt%), solution treated and overaged - precipitation hardening
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 57 Micrograph 57 : Al 96, Cu 4 (wt%), solution treated and overaged - precipitation hardening
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 657 Micrograph 657 : Al-4 wt% Cu, age hardened alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
20 μm
Link to full record for micrograph 658 Micrograph 658 : Al-4 wt% Cu, over aged alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 659 Micrograph 659 : Al-4 wt% Cu, over aged alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
200 μm