Categories > Metal or alloy > Ti-Al-V > Ti, Al 6, V 4 (wt%) > Keyword: titanium
2 micrographs available, ordered by micrograph number.
![]() |
Micrograph
54
:
Ti, Al 6, V 4 (wt%), Widmanstätten microstructure System: Ti-Al-V, Composition: Ti, Al 6, V 4 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
55
:
Ti, Al 6, V 4 (wt%), Widmanstätten microstructure System: Ti-Al-V, Composition: Ti, Al 6, V 4 (wt%) Reflected light microscopy 80 μm |