Browse the Library
Categories > Metal or alloy > Bi-Sn > Reflected light microscopy
3 micrographs available, ordered by micrograph number.
Micrograph
858
:
Bi 40wt%, Sn 60wt% System: Bi-Sn, Composition: Bi 40, Sn 60 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
859
:
Bi 60wt%, Sn 40wt% System: Bi-Sn, Composition: Bi 60, Sn 40 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
860
:
Bi 80wt%, Sn 20wt% System: Bi-Sn, Composition: Bi 80, Sn 20 (wt%) Reflected light microscopy 100 μm |
Help is available on browsing.