Link to full record for micrograph 70 Micrograph 70 : Silal
System: Fe-C-X, Composition: Fe, C 3.0, Si 6, Mn 0.7, P 0.3, S 0.1 (wt% typical) (Silal)
Reflected light microscopy
200 μm
Link to full record for micrograph 71 Micrograph 71 : Silal
System: Fe-C-X, Composition: Fe, C 3.0, Si 6, Mn 0.7, P 0.3, S 0.1 (wt% typical) (Silal)
Reflected light microscopy
80 μm
Link to full record for micrograph 72 Micrograph 72 : Ni-hard iron
System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron)
Reflected light microscopy
400 μm
Link to full record for micrograph 73 Micrograph 73 : Ni-hard iron
System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron)
Reflected light microscopy
80 μm
Link to full record for micrograph 420 Micrograph 420 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 421 Micrograph 421 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 422 Micrograph 422 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 423 Micrograph 423 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 424 Micrograph 424 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 425 Micrograph 425 : Cu 70, Zn 30 (wt%) (pure) brass, dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) (pure)
Reflected light microscopy
800 μm