Link to full record for micrograph 69 Micrograph 69 : Grey cast iron core with white cast iron periphery
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
40 μm
Link to full record for micrograph 70 Micrograph 70 : Silal
System: Fe-C-X, Composition: Fe, C 3.0, Si 6, Mn 0.7, P 0.3, S 0.1 (wt% typical) (Silal)
Reflected light microscopy
200 μm
Link to full record for micrograph 71 Micrograph 71 : Silal
System: Fe-C-X, Composition: Fe, C 3.0, Si 6, Mn 0.7, P 0.3, S 0.1 (wt% typical) (Silal)
Reflected light microscopy
80 μm
Link to full record for micrograph 72 Micrograph 72 : Ni-hard iron
System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron)
Reflected light microscopy
400 μm
Link to full record for micrograph 73 Micrograph 73 : Ni-hard iron
System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron)
Reflected light microscopy
80 μm
Link to full record for micrograph 201 Micrograph 201 : Normalised low carbon steel, showing directionality
System: Fe-C-X, Composition: Wrought iron (plain carbon steel)
Reflected light microscopy
400 μm
Link to full record for micrograph 202 Micrograph 202 : Normalised low carbon steel, showing directionality
System: Fe-C-X, Composition: Wrought iron (plain carbon steel)
Reflected light microscopy
200 μm
Link to full record for micrograph 203 Micrograph 203 : Normalised low carbon manganese steel, showing directionality
System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 204 Micrograph 204 : Normalised low carbon manganese steel, showing directionality
System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 205 Micrograph 205 : Normalised low carbon manganese steel, taken transverse to directionality
System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%)
Reflected light microscopy
400 μm