Categories > Metal or alloy > Reflected light microscopy > Keyword: aluminium

27 micrographs available, ordered by micrograph number.


Showing 11 - 20 of 27 micrographs Page 1 2 3 | Previous | Next

Link to full record for micrograph 59 Micrograph 59 : Al 88, Si 12 (wt%), eutectic alloy
System: Al-Si, Composition: Al 88, Si 12 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 60 Micrograph 60 : Al, Si 12, Na 0.02 (wt%), eutectic alloy - refined microstructure
System: Al-Si-Na, Composition: Al, Si 12, Na 0.02 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 61 Micrograph 61 : Al, Si 12, Na 0.02 (wt%), eutectic alloy - refined microstructure
System: Al-Si-Na, Composition: Al, Si 12, Na 0.02 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 613 Micrograph 613 : Facetted aluminium dendrites
System: Al-Sn, Composition: Al 15, Sn 85 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 615 Micrograph 615 : Cross-section of an aluminium casting
System: Al, Composition: Commercial purity (99.5%)
Reflected light microscopy
10 mm
Link to full record for micrograph 656 Micrograph 656 : Al, commercial purity
System: Al, Composition: Not specified
Reflected light microscopy
10 mm
Link to full record for micrograph 657 Micrograph 657 : Al-4 wt% Cu, age hardened alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
20 μm
Link to full record for micrograph 658 Micrograph 658 : Al-4 wt% Cu, over aged alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 659 Micrograph 659 : Al-4 wt% Cu, over aged alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 660 Micrograph 660 : Al-4 wt% Cu, over aged alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
100 μm