509 micrographs available, ordered by micrograph number.
Showing 481 - 490 of 509 micrographs | Page 1 .. 45 46 47 48 49 50 51 | Previous | Next |
Micrograph
918
:
Dasht-e-Kavir, Saghand - Posht-e-Badam. Copper slag System: Cu production, Composition: Not specified Reflected light microscopy 100 μm |
|
Micrograph
919
:
Hunsrueck mountain, Germany. Iron slag System: Fe production, Composition: Not specified Reflected light microscopy 200 μm |
|
Micrograph
920
:
Joldelund, Germany. Iron slag System: Fe production, Composition: Not specified Reflected light microscopy 500 μm |
|
Micrograph
921
:
Monte Romero, Huelva district, Spain. Phoenician, preroman silverproduction from complex ores. System: Pre-Roman Ag production, Composition: Not specified Reflected light microscopy 200 μm |
|
Micrograph
923
:
Dilbrecht Westerwald, Germany. Iron slag System: Fe production, Composition: Not specified Reflected light microscopy 200 μm |
|
Micrograph
928
:
Edo time japanese sword System: Ti-Al-V, Composition: Ti, Al 6, V 4 (wt%) Reflected light microscopy 2 mm |
|
Micrograph
929
:
Edo time japanese sword System: Ti-Al-V, Composition: Ti, Al 6, V 4 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
931
:
Afunfun, Niger. Melilith-pyroxene-copper slag System: Cu production, Composition: Not specified Reflected light microscopy 200 μm |
|
Micrograph
932
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag (hallstatt - latène) System: Smithing slag, Composition: Not specified Reflected light microscopy 500 μm |
|
Micrograph
934
:
Experimental iron production, Ph. Andrieux, Paris System: Fe production, Composition: Not specified Reflected light microscopy 500 μm |
Showing 481 - 490 of 509 micrographs | Page 1 .. 45 46 47 48 49 50 51 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.