Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

DoITPoMS Micrograph Library Full Record for Micrograph 919

Full Record for Micrograph 919

Micrograph no
919
Brief description
Hunsrueck mountain, Germany. Iron slag
Keywords
Categories
System
Fe production
Composition
Not specified
Standard codes
Reaction
Processing
Applications
Sample preparation
Thin slide, double sided polished. 30-40 µm
Technique
Reflected light microscopy
Length bar
200 μm
Further information
Contributor
Dr Ingo Keesmann
Organisation
Johannes Gutenberg-Universitat Mainz
Date
15/10/10
Licence for re-use
DoITPoMS standard terms of use