Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page
![micrograph index montage](images/montage.jpg)
Composition
11 micrographs for composition Not specified (System: Fe production), ordered by micrograph number.
Showing 1 - 10 of 11 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
909
:
Joldelund, Germany. Iron slag System: Fe production, Composition: Not specified Transmitted light microscopy 1 mm |
![]() |
Micrograph
919
:
Hunsrueck mountain, Germany. Iron slag System: Fe production, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
920
:
Joldelund, Germany. Iron slag System: Fe production, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
923
:
Dilbrecht Westerwald, Germany. Iron slag System: Fe production, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
925
:
Wissenbach, Westerwald, Germany. Iron slag System: Fe production, Composition: Not specified Transmitted light microscopy 200 μm |
![]() |
Micrograph
926
:
Wissenbach, Westerwald, Germany. Iron slag System: Fe production, Composition: Not specified Transmitted light microscopy 500 μm |
![]() |
Micrograph
927
:
Wissenbach, Westerwald, Germany. Iron slag System: Fe production, Composition: Not specified Transmitted light microscopy 500 μm |
![]() |
Micrograph
934
:
Experimental iron production, Ph. Andrieux, Paris System: Fe production, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
950
:
Haus Rhade, Sauerland, Germany. Subrecent Fe-production System: Fe production, Composition: Not specified Transmitted light microscopy 1 mm |
![]() |
Micrograph
951
:
Haus Rhade, Sauerland, Germany. Subrecent Fe-production System: Fe production, Composition: Not specified Transmitted light microscopy 500 μm |
Showing 1 - 10 of 11 micrographs | Page 1 2 | Previous | Next |