Link to full record for micrograph 156 Micrograph 156 : Roll-bonded aluminium alloy diffusion couple annealed for 30 minutes at 600ºC.
System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%)
Cross-polarised light microscopy
400 μm
Link to full record for micrograph 157 Micrograph 157 : Roll-bonded aluminium alloy diffusion couple annealed for 60 minutes at 600ºC.
System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%)
Cross-polarised light microscopy
750 μm
Link to full record for micrograph 158 Micrograph 158 : Roll-bonded aluminium alloy diffusion couple in the as-rolled condition.
System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%)
Cross-polarised light microscopy
400 μm
Link to full record for micrograph 159 Micrograph 159 : Roll-bonded aluminium alloy diffusion couple in the as-rolled condition.
System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%)
Cross-polarised light microscopy
2 mm
Link to full record for micrograph 710 Micrograph 710 : Wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute); refined with TiB2 particles. Deformation of grain structure is due to cutting of sample with scissors.
System: Al-Mg-Fe-Si, Composition: Not specified
Cross-polarised light microscopy
400 μm
Link to full record for micrograph 711 Micrograph 711 : As-cast wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute). No addition of grain refinement particles (e.g. TiB2).
System: Al-Mg-Fe-Si, Composition: Not specified
Cross-polarised light microscopy
1 mm
Link to full record for micrograph 712 Micrograph 712 : As-cast wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute). Addition of TiB2 particles facilitates the formation of a fine, equiaxed grain structure (grain refinement).
System: Al-Mg-Fe-Si, Composition: Not specified
Cross-polarised light microscopy
400 μm