Browse the Library
Categories > Metal or alloy > Transmission electron microscopy (TEM)
27 micrographs available, ordered by micrograph number.
Showing 21 - 27 of 27 micrographs | Page 1 2 3 | Previous | Next |
Micrograph
824
:
Martensitic steel tempered, with precipitation of Mo2C in ferrite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 1 μm |
|
Micrograph
827
:
Martensitic steel quenched then tempered System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 1 μm |
|
Micrograph
828
:
Martensitic steel tempered, with precipitation of Mo2C on dislocations in ferrite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 500 nm |
|
Micrograph
829
:
Martensitic steel quenched then tempered, with precipitation of Mo2C on dislocations in ferrite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 500 nm |
|
Micrograph
830
:
Martensitic steel tempered, with precipitation of Mo2C on dislocations System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 2 μm |
|
Micrograph
832
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 200 nm |
|
Micrograph
835
:
Martensitic steel tempered, with precipitation of Mo2C System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 1 μm |
Showing 21 - 27 of 27 micrographs | Page 1 2 3 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.