Browse the Library
Categories > Polymer composite
11 micrographs available, ordered by micrograph number.
| Showing 1 - 10 of 11 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
557
:
High Impact Polystyrene (HIPS) System: High Impact Polystyrene (HIPS), Composition: PS - 15%PB Transmitted light microscopy 10 μm |
![]() |
Micrograph
558
:
High Impact Polystyrene (HIPS) System: High Impact Polystyrene (HIPS), Composition: PS - 35%PB Transmitted light microscopy 20 μm |
![]() |
Micrograph
596
:
Glass-fibre reinforced polymer System: Polypropylene (PP), Composition: Polypropylene with 15% glass fibres Reflected light microscopy 400 μm |
![]() |
Micrograph
597
:
Frozen stress photoelastic fringe pattern during fibre pushout System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre' Cross-polarised light microscopy 6 mm |
![]() |
Micrograph
598
:
Frozen stress photoelastic assessment of load distribution around a cylinder System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre' Cross-polarised light microscopy 6 mm |
![]() |
Micrograph
599
:
Frozen stress photoelastic assessment of load distribution around an ellipsoid System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with ellipsoid CT200/HT901 'particle' Cross-polarised light microscopy 6 mm |
![]() |
Micrograph
618
:
Fracture surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 600 μm |
![]() |
Micrograph
619
:
Tensile failure surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
![]() |
Micrograph
620
:
Kevlar fibre composite fracture surface System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix Scanning electron microscopy (SEM) 600 μm |
![]() |
Micrograph
621
:
Kevlar fibre composite shear surface System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |