Browse the Library
Categories > Foam > Keyword: composite material
12 micrographs available, ordered by micrograph number.
| Showing 1 - 10 of 12 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
579
:
SEM image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified Scanning electron microscopy (SEM) 800 μm |
![]() |
Micrograph
580
:
High magnification SEM image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified Scanning electron microscopy (SEM) 160 μm |
![]() |
Micrograph
581
:
X-ray tomography image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified X-ray tomography 1.5 mm |
![]() |
Micrograph
582
:
Low magnification SEM image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified Scanning electron microscopy (SEM) 4 mm |
![]() |
Micrograph
629
:
FORMGRIP closed cell aluminium foam System: Al, Composition: Not specified Photography (no microscope) 6 mm |
![]() |
Micrograph
630
:
FOAMCARP closed cell aluminium foam System: Al, Composition: Not specified Photography (no microscope) 6 mm |
![]() |
Micrograph
631
:
Coarse open celled aluminium foam produced by infiltration of sintered salt (FOAM-U-LIKE) System: Al, Composition: Not specified Photography (no microscope) 6 mm |
![]() |
Micrograph
632
:
Open-celled aluminium foam System: Al, Composition: Not specified Photography (no microscope) 8 mm |
![]() |
Micrograph
633
:
Cross-section of an aluminium foam slab produced by gas injection System: Al, Composition: Not specified Photography (no microscope) 10 mm |
![]() |
Micrograph
634
:
Solid-gas eutectic solidification (Gasar) aluminium foam System: Al, Composition: Not specified Photography (no microscope) 120 μm |