Categories > Fracture
41 micrographs available, ordered by micrograph number.
| Showing 31 - 40 of 41 micrographs | Page 1 2 3 4 5 | Previous | Next |
![]() |
Micrograph
618
:
Fracture surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 600 μm |
![]() |
Micrograph
619
:
Tensile failure surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
![]() |
Micrograph
620
:
Kevlar fibre composite fracture surface System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix Scanning electron microscopy (SEM) 600 μm |
![]() |
Micrograph
621
:
Kevlar fibre composite shear surface System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
![]() |
Micrograph
622
:
Kevlar fibre composite shear surface System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
![]() |
Micrograph
626
:
Glass fibre reinforced thermoplastic matrix composite System: Glass fibre composite, Composition: Polypropylene matrix with glass fibre Scanning electron microscopy (SEM) 60 μm |
![]() |
Micrograph
627
:
Glass fibre reinforced thermoplastic matrix composite System: Glass fibre composite, Composition: Polypropylene matrix with glass fibre Scanning electron microscopy (SEM) 200 μm |
![]() |
Micrograph
640
:
Fracture surface in a liquid crystalline polymer, oriented by a magnetic field System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14401 Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
641
:
Fracture surface in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14401 Scanning electron microscopy (SEM) 12 μm |
![]() |
Micrograph
642
:
Fracture surface in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14402 Scanning electron microscopy (SEM) 12 μm |