Link to full record for micrograph 137 Micrograph 137 : Al-Mg-Si, failed through microvoid coalescence.
System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016)
Scanning electron microscopy (SEM)
40 μm
Link to full record for micrograph 138 Micrograph 138 : Al-Mg-Si, failed through microvoid coalescence.
System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016)
Scanning electron microscopy (SEM)
40 μm
Link to full record for micrograph 139 Micrograph 139 : Al-Mg-Si, failed through microvoid coalescence.
System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016)
Scanning electron microscopy (SEM)
40 μm
Link to full record for micrograph 140 Micrograph 140 : Al-Mg-Si, failed through microvoid coalescence.
System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016)
Scanning electron microscopy (SEM)
40 μm
Link to full record for micrograph 141 Micrograph 141 : Al-Mg-Si, failed through microvoid coalescence.
System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016)
Scanning electron microscopy (SEM)
40 μm