Micrograph
550
:
Micrograph showing the complex chemical reactions which arise at fibre-matrix interfaces in a fibre reinforced magnesium aluminosilicate ceramic subjected to oxidation System: SiC fibre-reinforced magnesium aluminosilicate, Composition: Not specified Bright-field TEM 300 nm |