Categories > Ceramic > Not specified > Keyword: nanotube

4 micrographs available, ordered by micrograph number.


Link to full record for micrograph 561 Micrograph 561 : Ordered film of carbon nanotubes
System: Carbon nanotube, Composition: Not specified
Field emission gun scanning electron microscopy (FEGSEM)
400 nm
Link to full record for micrograph 562 Micrograph 562 : Multi-walled carbon nanotube
System: Carbon nanotube, Composition: Not specified
Transmission electron microscopy (TEM)
3.2 nm
Link to full record for micrograph 564 Micrograph 564 : Aligned array of nanotubes
System: Carbon nanotube, Composition: Not specified
Scanning electron microscopy (SEM)
25 μm
Link to full record for micrograph 565 Micrograph 565 : Vapour-grown carbon nanotubes
System: Carbon nanotube, Composition: Not specified
Scanning electron microscopy (SEM)
5 μm