Categories > Ceramic > Terracotta is composed of mixtures of fired grog and clay. > Reflected light microscopy > Keyword: terracotta

3 micrographs available, ordered by micrograph number.


Link to full record for micrograph 177 Micrograph 177 : Terracotta pottery
System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay.
Reflected light microscopy
200 μm
Link to full record for micrograph 178 Micrograph 178 : Terracotta pottery, showing the glaze on the surface
System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay.
Reflected light microscopy
100 μm
Link to full record for micrograph 179 Micrograph 179 : Terracotta pottery, showing the glaze on the surface
System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay.
Reflected light microscopy
250 μm