Categories > Ceramic > Mostly clay (which consists of alumina and silica) > Keyword: vitrification

2 micrographs available, ordered by micrograph number.


Link to full record for micrograph 187 Micrograph 187 : Part of a Denby pottery mug, showing the glaze on the surface
System: Al2O3-SiO2, Composition: Mostly clay (which consists of alumina and silica)
Reflected light microscopy
200 μm
Link to full record for micrograph 188 Micrograph 188 : Part of a Denby pottery mug
System: Al2O3-SiO2, Composition: Mostly clay (which consists of alumina and silica)
Reflected light microscopy
200 μm