Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Ceramic > Keyword: alumina
10 micrographs available, ordered by micrograph number.
![]() |
Micrograph
84
:
Alumina System: Alumina, Composition: Not specified Reflected light microscopy 800 μm |
![]() |
Micrograph
85
:
Alumina System: Alumina, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
150
:
Alumina-zirconia-silica (AZS) refractory brick System: Al2O3-ZrO2-SiO2, Composition: Al2O3 50, ZrO2 32, SiO2 15 (wt%), + trace alkalis Reflected light microscopy 300 μm |
![]() |
Micrograph
151
:
Alumina-graphite brick System: Al2O3-C-Si, Composition: Al2O3, C up to 30 (wt%), Si few% Reflected light microscopy 400 μm |
![]() |
Micrograph
172
:
Bone china (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
173
:
Bone china, showing the glaze on the surface (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
174
:
Bone china (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
195
:
Zirconia Toughened Alumina (ZTA) System: ZrO2-Al2O3, Composition: ZrO2 5-30, Al2O3 70-95 (wt%) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 10 μm |
![]() |
Micrograph
198
:
96% Alumina System: Al2O3, Composition: Al2O3 96%, remainder MgO, CaO, SiO2 Reflected light microscopy 250 μm |
![]() |
Micrograph
199
:
BaTiO3 Temperature-stable dielectric capacitor System: BaTiO3 + other oxides such as Nb2O5, Bi2O3, Composition: BaTiO3 95-97 (wt%) Bright-field TEM 1 μm |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.