Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Ceramic > Keyword: silicon carbide
11 micrographs available, ordered by micrograph number.
| Showing 1 - 10 of 11 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
185
:
Silicon Nitride-bonded Silicon Carbide System: Silicon nitride-bonded silicon carbide, Composition: Particles of SiC in a reaction-bonded Si3N4 matrix Reflected light microscopy 250 μm |
![]() |
Micrograph
186
:
Silicon Carbide from within a Silicon Nitride-bonded Silicon Carbide sample System: Silicon nitride-bonded silicon carbide, Composition: Particles of SiC in a reaction-bonded Si3N4 matrix Reflected light microscopy 25 μm |
![]() |
Micrograph
546
:
Delamination cracks seen in h-BN particles subjected to compressive stress in the (0001) planes (within a silicon nitride particulate-reinforced silicon carbide composite) System: Si3N4-SiC composite, Composition: Not specified High resolution electron microscopy (HREM) 10 nm |
![]() |
Micrograph
547
:
h-BN inclusion (precipitate) in a b-Si3N4 grain (within a silicon nitride particulate-reinforced silicon carbide composite) System: Si3N4-SiC composite, Composition: Not specified High resolution electron microscopy (HREM) 20 nm |
![]() |
Micrograph
549
:
Misoriented interphase boundary between h-BN (precipitate) and SiC grains (within a silicon nitride particulate-reinforced silicon carbide composite) System: Si3N4-SiC composite, Composition: Not specified High resolution electron microscopy (HREM) 1.2 nm |
![]() |
Micrograph
551
:
A regularly stepped interface boundary between h-BN (precipitate) and Si3N4 grains (within a silicon nitride particulate-reinforced silicon carbide composite) System: Si3N4-SiC composite, Composition: Not specified High resolution electron microscopy (HREM) 10 nm |
![]() |
Micrograph
552
:
An amorphous phase trapped at a triple junction between Si3N4 grains (within a silicon nitride particulate-reinforced silicon carbide composite). System: Si3N4-SiC composite, Composition: Not specified High resolution electron microscopy (HREM) 20 nm |
![]() |
Micrograph
553
:
Image of part of a crystalline triple junction between SiC grains (within a silicon nitride particulate-reinforced silicon carbide composite) System: Si3N4-SiC composite, Composition: Not specified High resolution electron microscopy (HREM) 6 nm |
![]() |
Micrograph
554
:
Silicon carbide System: SiC, Composition: Not specified Photography (no microscope) 10 mm |
![]() |
Micrograph
691
:
Silicon carbide System: SiC, Composition: Not specified Reflected light microscopy 100 μm |
| Showing 1 - 10 of 11 micrographs | Page 1 2 | Previous | Next |
Help is available on browsing.