Categories > Ceramic > Reflected light microscopy > Keyword: alumina
5 micrographs available, ordered by micrograph number.
Micrograph
84
:
Alumina System: Alumina, Composition: Not specified Reflected light microscopy 800 μm |
|
Micrograph
85
:
Alumina System: Alumina, Composition: Not specified Reflected light microscopy 200 μm |
|
Micrograph
150
:
Alumina-zirconia-silica (AZS) refractory brick System: Al2O3-ZrO2-SiO2, Composition: Al2O3 50, ZrO2 32, SiO2 15 (wt%), + trace alkalis Reflected light microscopy 300 μm |
|
Micrograph
151
:
Alumina-graphite brick System: Al2O3-C-Si, Composition: Al2O3, C up to 30 (wt%), Si few% Reflected light microscopy 400 μm |
|
Micrograph
198
:
96% Alumina System: Al2O3, Composition: Al2O3 96%, remainder MgO, CaO, SiO2 Reflected light microscopy 250 μm |