Categories > Composite > Commercial purity (99.5%) + 13 micron alumina spheroids
1 micrograph available, ordered by micrograph number.
![]() |
Micrograph
611
:
Section of a metal matrix composite (MMC) after extrusion and annealing System: Al, Composition: Commercial purity (99.5%) + 13 micron alumina spheroids Reflected light microscopy, polarised 40 μm |