Categories > Composite > Keyword: fibre
9 micrographs available, ordered by micrograph number.
![]() |
Micrograph
596
:
Glass-fibre reinforced polymer System: Polypropylene (PP), Composition: Polypropylene with 15% glass fibres Reflected light microscopy 400 μm |
![]() |
Micrograph
597
:
Frozen stress photoelastic fringe pattern during fibre pushout System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre' Cross-polarised light microscopy 6 mm |
![]() |
Micrograph
602
:
Section of a metal matrix composite (MMC) System: Al-Mg, Composition: Al, Mg 2.5 (wt%), with Al2O3 (10 vol%) Reflected light microscopy, polarised 80 μm |
![]() |
Micrograph
603
:
Section of a metal matrix composite (MMC) System: Al-Mg, Composition: Al, Mg 2.5 (wt%), with Al2O3 (5 vol%) Reflected light microscopy, polarised 80 μm |
![]() |
Micrograph
618
:
Fracture surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 600 μm |
![]() |
Micrograph
619
:
Tensile failure surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
![]() |
Micrograph
620
:
Kevlar fibre composite fracture surface System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix Scanning electron microscopy (SEM) 600 μm |
![]() |
Micrograph
621
:
Kevlar fibre composite shear surface System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
![]() |
Micrograph
622
:
Kevlar fibre composite shear surface System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
Help is available on browsing.