Browse the Library
Categories > Composite > Scanning electron microscopy (SEM)
11 micrographs available, ordered by micrograph number.
| Showing 1 - 10 of 11 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
579
:
SEM image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified Scanning electron microscopy (SEM) 800 μm |
![]() |
Micrograph
580
:
High magnification SEM image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified Scanning electron microscopy (SEM) 160 μm |
![]() |
Micrograph
582
:
Low magnification SEM image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified Scanning electron microscopy (SEM) 4 mm |
![]() |
Micrograph
616
:
Cavity formation in a tensile loaded alumina particulate composite System: Al, Composition: Commercial purity (99.5%) + 15 micron angular alumina particles Scanning electron microscopy (SEM) 80 μm |
![]() |
Micrograph
618
:
Fracture surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 600 μm |
![]() |
Micrograph
619
:
Tensile failure surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
![]() |
Micrograph
620
:
Kevlar fibre composite fracture surface System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix Scanning electron microscopy (SEM) 600 μm |
![]() |
Micrograph
621
:
Kevlar fibre composite shear surface System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
![]() |
Micrograph
622
:
Kevlar fibre composite shear surface System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
![]() |
Micrograph
626
:
Glass fibre reinforced thermoplastic matrix composite System: Glass fibre composite, Composition: Polypropylene matrix with glass fibre Scanning electron microscopy (SEM) 60 μm |