Browse the Library
Categories > Composite > Reflected light microscopy > Keyword: ceramic
5 micrographs available, ordered by micrograph number.
Micrograph
151
:
Alumina-graphite brick System: Al2O3-C-Si, Composition: Al2O3, C up to 30 (wt%), Si few% Reflected light microscopy 400 μm |
|
Micrograph
175
:
Concrete from a commercial paving slab System: Concrete, Composition: Aggregate, cement, water Reflected light microscopy 100 μm |
|
Micrograph
176
:
Concrete from a commercial paving slab System: Concrete, Composition: Aggregate, cement, water Reflected light microscopy 250 μm |
|
Micrograph
193
:
MgO-C Refractory Brick System: MgO-C, Composition: MgO 50-90, C 8-37 (wt%), remainder Al, Si metal addition Reflected light microscopy 200 μm |
|
Micrograph
194
:
MgO-C Refractory Brick System: MgO-C, Composition: MgO 50-90, C 8-37 (wt%), remainder Al, Si metal addition Reflected light microscopy 200 μm |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.