Browse the Library
Categories > Polymer > Keyword: fibre
11 micrographs available, ordered by micrograph number.
| Showing 1 - 10 of 11 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
594
:
Carbon string System: C, Composition: Not specified Scanning electron microscopy (SEM) 400 μm |
![]() |
Micrograph
596
:
Glass-fibre reinforced polymer System: Polypropylene (PP), Composition: Polypropylene with 15% glass fibres Reflected light microscopy 400 μm |
![]() |
Micrograph
597
:
Frozen stress photoelastic fringe pattern during fibre pushout System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre' Cross-polarised light microscopy 6 mm |
![]() |
Micrograph
618
:
Fracture surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 600 μm |
![]() |
Micrograph
619
:
Tensile failure surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
![]() |
Micrograph
620
:
Kevlar fibre composite fracture surface System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix Scanning electron microscopy (SEM) 600 μm |
![]() |
Micrograph
621
:
Kevlar fibre composite shear surface System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
![]() |
Micrograph
622
:
Kevlar fibre composite shear surface System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
![]() |
Micrograph
640
:
Fracture surface in a liquid crystalline polymer, oriented by a magnetic field System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14401 Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
641
:
Fracture surface in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14401 Scanning electron microscopy (SEM) 12 μm |