Browse the Library
Categories > Polymer > Polystyrene (PS)
11 micrographs available, ordered by micrograph number.
| Showing 1 - 10 of 11 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
560
:
Crazing near a fracture surface in polystyrene System: Polystyrene (PS), Composition: Not specified Photography (no microscope) 10 mm |
![]() |
Micrograph
569
:
Injection-moulded polystyrene ruler System: Polystyrene (PS), Composition: Not specified Cross-polarised light microscopy 11 mm |
![]() |
Micrograph
574
:
Injection-moulded polystyrene (PS) case System: Polystyrene (PS), Composition: Not specified Cross-polarised light microscopy 14 mm |
![]() |
Micrograph
575
:
Injection-moulded protractor System: Polystyrene (PS), Composition: Not specified Cross-polarised light microscopy 6 mm |
![]() |
Micrograph
576
:
Injection-moulded protractor System: Polystyrene (PS), Composition: Not specified Cross-polarised light microscopy 30 mm |
![]() |
Micrograph
586
:
Fracture surface in polystyrene System: Polystyrene (PS), Composition: Not specified Scanning electron microscopy (SEM) 160 μm |
![]() |
Micrograph
587
:
Parabolic beach marks on a polystyrene fracture surface System: Polystyrene (PS), Composition: Not specified Scanning electron microscopy (SEM) 80 μm |
![]() |
Micrograph
588
:
Beach marks on a polystyrene fracture surface System: Polystyrene (PS), Composition: Not specified Scanning electron microscopy (SEM) 50 μm |
![]() |
Micrograph
589
:
Remnants of crazes on a polystyrene fracture surface System: Polystyrene (PS), Composition: Not specified Scanning electron microscopy (SEM) 8 μm |
![]() |
Micrograph
851
:
Polystyrene System: Polystyrene (PS), Composition: Polystyrene Atomic force microscopy (AFM) 2 μm |