Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Polymer > Atomic force microscopy (AFM)
10 micrographs available, ordered by micrograph number.
![]() |
Micrograph
646
:
Spherulite growth imaged by atomic force microscopy (AFM) System: Polyhydroxybutyrate (PHB), Composition: Not specified Atomic force microscopy (AFM) 500 nm |
![]() |
Micrograph
647
:
A spherulite imaged by atomic force microscopy (AFM) System: Polyhydroxybutyrate (PHB), Composition: Not specified Atomic force microscopy (AFM) 3 μm |
![]() |
Micrograph
648
:
A spherulite imaged by atomic force microscopy (AFM) System: Polyhydroxybutyrate (PHB), Composition: Not specified Atomic force microscopy (AFM) 2 μm |
![]() |
Micrograph
649
:
An image of an alkane crystal taken by AFM System: Alkane, Composition: C36H74 Atomic force microscopy (AFM) 30 μm |
![]() |
Micrograph
851
:
Polystyrene System: Polystyrene (PS), Composition: Polystyrene Atomic force microscopy (AFM) 2 μm |
![]() |
Micrograph
852
:
Polystyrene System: Polystyrene (PS), Composition: Polystyrene Atomic force microscopy (AFM) 200 nm |
![]() |
Micrograph
853
:
Colloidal polymethyl methacrylate System: Poly methyl methacrylate, Composition: Poly methyl methacrylate Atomic force microscopy (AFM) 200 nm |
![]() |
Micrograph
861
:
Carbon System: C, Composition: Carbon Atomic force microscopy (AFM) 2 μm |
![]() |
Micrograph
862
:
Carbon System: C, Composition: Carbon Atomic force microscopy (AFM) 1 μm |
![]() |
Micrograph
863
:
Carbon System: C, Composition: Carbon Atomic force microscopy (AFM) 100 nm |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.