Micrograph
555
:
Banded spherulites in a blend of polyethtylenes System: Polyethylene (PE), Composition: LPE:BPE 1:3 Transmission electron microscopy (TEM) 200 nm |
![]() |
Micrograph
556
:
Sheaf-like arrangement of lamellae in a blend of polyethylenes System: Polyethylene (PE), Composition: LPE:BPE 3:1 Transmission electron microscopy (TEM) 200 nm |
![]() |
Micrograph
562
:
Multi-walled carbon nanotube System: Carbon nanotube, Composition: Not specified Transmission electron microscopy (TEM) 3.2 nm |
![]() |
Micrograph
645
:
An image of a single crystal alkane System: Alkane, Composition: C294H590 Transmission electron microscopy (TEM) 2.4 μm |