Categories > Polymer > Liquid crystalline polymer > Semi-flexible LCP, Cl-8 > Keyword: dislocation

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 638 Micrograph 638 : Disclinations in a smectic LCP, revealed by decoration
System: Liquid crystalline polymer, Composition: Semi-flexible LCP, Cl-8
Cross-polarised light microscopy
10 μm