Browse the Library
Categories > Polymer > Cross-polarised light microscopy > Keyword: polymer
23 micrographs available, ordered by micrograph number.
Showing 11 - 20 of 23 micrographs | Page 1 2 3 | Previous | Next |
Micrograph
576
:
Injection-moulded protractor System: Polystyrene (PS), Composition: Not specified Cross-polarised light microscopy 30 mm |
|
Micrograph
577
:
Injection-moulded polypropylene (PP) hinge System: Polypropylene (PP), Composition: Not specified Cross-polarised light microscopy 1.4 mm |
|
Micrograph
578
:
Sprue in a sample of polypropylene (PP) System: Polypropylene (PP), Composition: Not specified Cross-polarised light microscopy 10 mm |
|
Micrograph
597
:
Frozen stress photoelastic fringe pattern during fibre pushout System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre' Cross-polarised light microscopy 6 mm |
|
Micrograph
598
:
Frozen stress photoelastic assessment of load distribution around a cylinder System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre' Cross-polarised light microscopy 6 mm |
|
Micrograph
599
:
Frozen stress photoelastic assessment of load distribution around an ellipsoid System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with ellipsoid CT200/HT901 'particle' Cross-polarised light microscopy 6 mm |
|
Micrograph
600
:
Spherulite in poly-3-hydroxy butyrate (PHB) System: Polyhydroxybutyrate (PHB), Composition: Not specified Cross-polarised light microscopy 1 μm |
|
Micrograph
601
:
Spherulites in in poly-3-hydroxy butyrate (PHB) System: Polyhydroxybutyrate (PHB), Composition: Not specified Cross-polarised light microscopy 240 nm |
|
Micrograph
612
:
Nematic liquid crystalline polymer System: Liquid crystalline polymer, Composition: K24 (4-cyano-4'-8-alkylbiphenyl) Cross-polarised light microscopy 100 μm |
|
Micrograph
625
:
Series of laser welds in amorphous PET System: Polyethylene terephthalate (PET), Composition: Amorphous polyethylene terephthalate (APET) Cross-polarised light microscopy 12 mm |
Showing 11 - 20 of 23 micrographs | Page 1 2 3 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.