Link to full record for micrograph 442 Micrograph 442 : Cu 60, Zn 40 (wt%) brass, Widmanstätten microstructure
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 443 Micrograph 443 : Commercial grade free machining brass - Widmanstätten microstructure
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) + Pb trace
Reflected light microscopy
400 μm
Link to full record for micrograph 444 Micrograph 444 : Commercial grade free machining brass - Widmanstätten microstructure
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) + Pb trace
Reflected light microscopy
200 μm
Link to full record for micrograph 445 Micrograph 445 : Cast and annealed 40 wt% Zn brass
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) + Pb trace
Reflected light microscopy
400 μm
Link to full record for micrograph 446 Micrograph 446 : Cast and annealed 40 wt% Zn brass
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) + Pb trace
Reflected light microscopy
200 μm
Link to full record for micrograph 447 Micrograph 447 : Cu 65, Zn 35 (wt%) B4 brass, chill cast
System: Cu-Zn, Composition: Cu 65, Zn 35 (wt%) (pure)
Reflected light microscopy
400 μm
Link to full record for micrograph 448 Micrograph 448 : Cu 65, Zn 35 (wt%) B4 brass, chill cast
System: Cu-Zn, Composition: Cu 65, Zn 35 (wt%) (pure)
Reflected light microscopy
200 μm
Link to full record for micrograph 449 Micrograph 449 : Cu 55, Zn 45 (wt%) brass, rapidly cooled
System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 450 Micrograph 450 : Cu 55, Zn 45 (wt%) brass, rapidly cooled
System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 451 Micrograph 451 : Cu 55, Zn 45 (wt%) brass, rapidly cooled
System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%)
Reflected light microscopy
100 μm