708 micrographs for category Metal or alloy:


Showing 421 - 430 of 708 micrographs Page 1 .. 40 41 42 43 44 45 46 .. 71 | Previous | Next

Link to full record for micrograph 605 Micrograph 605 : Fracture surface formed by hot tearing (solidification cracking)
System: Al, Composition: Commercial purity (99.5%)
Scanning electron microscopy (SEM)
40 μm
Link to full record for micrograph 607 Micrograph 607 : Fibre fracture in a metal matrix composite
System: Al, Composition: Commercial purity (99.5%)
Scanning electron microscopy (SEM)
4 μm
Link to full record for micrograph 608 Micrograph 608 : Channelling contrast TEM image of subgrains of extruded aluminium
System: Al, Composition: Commercial purity (99.5%)
Transmission electron microscopy (TEM)
600 nm
Link to full record for micrograph 609 Micrograph 609 : The grain structure of extruded aluminium
System: Al, Composition: Commercial purity (99.5%)
Reflected light microscopy, polarised
40 μm
Link to full record for micrograph 613 Micrograph 613 : Facetted aluminium dendrites
System: Al-Sn, Composition: Al 15, Sn 85 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 614 Micrograph 614 : Rapid solidification in an atomised droplet
System: Al-Mg, Composition: Al 90, Mg 10 (wt%)
Transmission electron microscopy (TEM)
500 nm
Link to full record for micrograph 615 Micrograph 615 : Cross-section of an aluminium casting
System: Al, Composition: Commercial purity (99.5%)
Reflected light microscopy
10 mm
Link to full record for micrograph 617 Micrograph 617 : Deeply etched Co-dendrites
System: Co-Sm-Cu, Composition: Co 70, Sm 10, Cu 20 (at%)
Scanning electron microscopy (SEM)
80 μm
Link to full record for micrograph 629 Micrograph 629 : FORMGRIP closed cell aluminium foam
System: Al, Composition: Not specified
Photography (no microscope)
6 mm
Link to full record for micrograph 630 Micrograph 630 : FOAMCARP closed cell aluminium foam
System: Al, Composition: Not specified
Photography (no microscope)
6 mm