Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Category
708 micrographs for category Metal or alloy:
| Showing 571 - 580 of 708 micrographs | Page 1 .. 55 56 57 58 59 60 61 .. 71 | Previous | Next |
![]() |
Micrograph
820
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Nb 5, C O.1 (wt%) Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
821
:
Austenitic stainless steel impact deformed at room temperature System: Fe-C-X, Composition: Fe, C 1.15, Mn 13 (wt%) Scanning electron microscopy (SEM) 2.5 μm |
![]() |
Micrograph
822
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Transmission electron microscopy (TEM) 400 nm |
![]() |
Micrograph
823
:
Martensitic steel tempered, with dislocation helices in ferrite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 1 μm |
![]() |
Micrograph
824
:
Martensitic steel tempered, with precipitation of Mo2C in ferrite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 1 μm |
![]() |
Micrograph
826
:
Austenitic stainless steel tempered, with Mo2 and M6C precipitates System: Fe-C-X, Composition: Fe, C 0.20, Mo 3.8, Ta 0.22 (wt%) Scanning electron microscopy (SEM) 2.5 μm |
![]() |
Micrograph
827
:
Martensitic steel quenched then tempered System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 1 μm |
![]() |
Micrograph
828
:
Martensitic steel tempered, with precipitation of Mo2C on dislocations in ferrite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 500 nm |
![]() |
Micrograph
829
:
Martensitic steel quenched then tempered, with precipitation of Mo2C on dislocations in ferrite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 500 nm |
![]() |
Micrograph
830
:
Martensitic steel tempered, with precipitation of Mo2C on dislocations System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 2 μm |
| Showing 571 - 580 of 708 micrographs | Page 1 .. 55 56 57 58 59 60 61 .. 71 | Previous | Next |