Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Category
708 micrographs for category Metal or alloy:
| Showing 651 - 660 of 708 micrographs | Page 1 .. 63 64 65 66 67 68 69 .. 71 | Previous | Next |
![]() |
Micrograph
918
:
Dasht-e-Kavir, Saghand - Posht-e-Badam. Copper slag System: Cu production, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
919
:
Hunsrueck mountain, Germany. Iron slag System: Fe production, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
920
:
Joldelund, Germany. Iron slag System: Fe production, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
921
:
Monte Romero, Huelva district, Spain. Phoenician, preroman silverproduction from complex ores. System: Pre-Roman Ag production, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
922
:
Monte Romero, Huelva district, Spain. Phoenician, preroman silver production from complex ores. System: Pre-Roman Ag production, Composition: Not specified Transmitted light microscopy 200 μm |
![]() |
Micrograph
923
:
Dilbrecht Westerwald, Germany. Iron slag System: Fe production, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
924
:
Monte Romero, Huelva district, Spain. Phoenician, preroman silver production from complex ores. System: Pre-Roman Ag production, Composition: Not specified Transmitted light microscopy 200 μm |
![]() |
Micrograph
925
:
Wissenbach, Westerwald, Germany. Iron slag System: Fe production, Composition: Not specified Transmitted light microscopy 200 μm |
![]() |
Micrograph
926
:
Wissenbach, Westerwald, Germany. Iron slag System: Fe production, Composition: Not specified Transmitted light microscopy 500 μm |
![]() |
Micrograph
927
:
Wissenbach, Westerwald, Germany. Iron slag System: Fe production, Composition: Not specified Transmitted light microscopy 500 μm |
| Showing 651 - 660 of 708 micrographs | Page 1 .. 63 64 65 66 67 68 69 .. 71 | Previous | Next |