41 micrographs for category Fracture:


Showing 31 - 40 of 41 micrographs Page 1 2 3 4 5 | Previous | Next

Link to full record for micrograph 618 Micrograph 618 : Fracture surface of a carbon fibre composite
System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
600 μm
Link to full record for micrograph 619 Micrograph 619 : Tensile failure surface of a carbon fibre composite
System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 620 Micrograph 620 : Kevlar fibre composite fracture surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
600 μm
Link to full record for micrograph 621 Micrograph 621 : Kevlar fibre composite shear surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 622 Micrograph 622 : Kevlar fibre composite shear surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 626 Micrograph 626 : Glass fibre reinforced thermoplastic matrix composite
System: Glass fibre composite, Composition: Polypropylene matrix with glass fibre
Scanning electron microscopy (SEM)
60 μm
Link to full record for micrograph 627 Micrograph 627 : Glass fibre reinforced thermoplastic matrix composite
System: Glass fibre composite, Composition: Polypropylene matrix with glass fibre
Scanning electron microscopy (SEM)
200 μm
Link to full record for micrograph 640 Micrograph 640 : Fracture surface in a liquid crystalline polymer, oriented by a magnetic field
System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14401
Scanning electron microscopy (SEM)
4 μm
Link to full record for micrograph 641 Micrograph 641 : Fracture surface in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14401
Scanning electron microscopy (SEM)
12 μm
Link to full record for micrograph 642 Micrograph 642 : Fracture surface in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14402
Scanning electron microscopy (SEM)
12 μm