80 micrographs for category Ceramic:


Showing 31 - 40 of 80 micrographs Page 1 2 3 4 5 6 7 8 | Previous | Next

Link to full record for micrograph 183 Micrograph 183 : Oven-to-tableware
System: Miscellaneous, Composition: Not specified
Transmitted polarised light microscopy
250 μm
Link to full record for micrograph 184 Micrograph 184 : Oven-to-tableware
System: Miscellaneous, Composition: Not specified
Transmitted polarised light microscopy
250 μm
Link to full record for micrograph 185 Micrograph 185 : Silicon Nitride-bonded Silicon Carbide
System: Silicon nitride-bonded silicon carbide, Composition: Particles of SiC in a reaction-bonded Si3N4 matrix
Reflected light microscopy
250 μm
Link to full record for micrograph 186 Micrograph 186 : Silicon Carbide from within a Silicon Nitride-bonded Silicon Carbide sample
System: Silicon nitride-bonded silicon carbide, Composition: Particles of SiC in a reaction-bonded Si3N4 matrix
Reflected light microscopy
25 μm
Link to full record for micrograph 187 Micrograph 187 : Part of a Denby pottery mug, showing the glaze on the surface
System: Al2O3-SiO2, Composition: Mostly clay (which consists of alumina and silica)
Reflected light microscopy
200 μm
Link to full record for micrograph 188 Micrograph 188 : Part of a Denby pottery mug
System: Al2O3-SiO2, Composition: Mostly clay (which consists of alumina and silica)
Reflected light microscopy
200 μm
Link to full record for micrograph 189 Micrograph 189 : Titanate ceramic for immobilising radioactive waste
System: Oxides + simulated fission products, Composition: Not specified
Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode
30 μm
Link to full record for micrograph 190 Micrograph 190 : Aluminous Electrical Porcelain
System: Triaxial (i.e. clay/flux/filler) porcelain, Composition: Ball clay 30 , china clay 10, potash feldspar 20, silica sand 20, calcined alumina 20 (wt%)
Scanning electron microscopy (SEM)
10 μm
Link to full record for micrograph 191 Micrograph 191 : Dolomite (Ca,Mg)(CO3)2
System: CaCO3-MgCO3, Composition: CaO 57, MgO 41 (wt%), + Fe2O3, SiO2 and Al2O3 (typical)
Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode
30 μm
Link to full record for micrograph 192 Micrograph 192 : Doloma, (Ca,Mg)O
System: (Ca,Mg)O, Composition: CaO 57, MgO 41 (wt%), + Fe2O3, SiO2 and Al2O3 (typical)
Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode
30 μm

Showing 31 - 40 of 80 micrographs Page 1 2 3 4 5 6 7 8 | Previous | Next