Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Category
77 micrographs for category Polymer:
| Showing 41 - 50 of 77 micrographs | Page 1 2 3 4 5 6 7 8 | Previous | Next |
![]() |
Micrograph
591
:
Crazing near a fracture surface in polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 80 μm |
![]() |
Micrograph
592
:
The tip of a craze in polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
593
:
Ductile tearing near a fracture surface in polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 100 μm |
![]() |
Micrograph
594
:
Carbon string System: C, Composition: Not specified Scanning electron microscopy (SEM) 400 μm |
![]() |
Micrograph
595
:
Thermoset case of an electrical plug System: Urea formaldehyde, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
596
:
Glass-fibre reinforced polymer System: Polypropylene (PP), Composition: Polypropylene with 15% glass fibres Reflected light microscopy 400 μm |
![]() |
Micrograph
597
:
Frozen stress photoelastic fringe pattern during fibre pushout System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre' Cross-polarised light microscopy 6 mm |
![]() |
Micrograph
598
:
Frozen stress photoelastic assessment of load distribution around a cylinder System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre' Cross-polarised light microscopy 6 mm |
![]() |
Micrograph
599
:
Frozen stress photoelastic assessment of load distribution around an ellipsoid System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with ellipsoid CT200/HT901 'particle' Cross-polarised light microscopy 6 mm |
![]() |
Micrograph
600
:
Spherulite in poly-3-hydroxy butyrate (PHB) System: Polyhydroxybutyrate (PHB), Composition: Not specified Cross-polarised light microscopy 1 μm |
| Showing 41 - 50 of 77 micrographs | Page 1 2 3 4 5 6 7 8 | Previous | Next |